Properties in Cured Condition (24h RT + 15h @ 60°C)
Property | Conditions | Test Method | Value | Units |
---|---|---|---|---|
Density | 25°C | ASTM D792 | 1.37 – 1.41 | g/ml |
Hardness | 25°C | ASTM D2240 | 85 – 90 (Shore A), 40 – 50 (Shore D) | – |
Glass Transition (Tg) | – | ASTM D3418 | -5 to +10 | °C |
Water Absorption (240h, RT) | – | – | 0.2 – 0.3 | % |
Water Absorption (2h, 100°C) | – | ASTM D570 | 0.8 – 1.0 | % |
Linear Thermal Expansion (Tg -10°C) | – | ASTM E831 | 70 – 80 | 10⁻⁶/°C |
Linear Thermal Expansion (Tg +10°C) | – | ASTM E831 | 160 – 180 | 10⁻⁶/°C |
Thermal Shock | 10 cycles | Olyphant | -40 to +170 | °C |
Flammability | – | UL94 | V0 (13 mm) | – |
Max Operating Temperature | – | UL746B | 130 | °C |
Thermal Conductivity | 25°C | ASTM C518 | 0.50 – 0.60 | W/(m·K) |
Dielectric Constant | 25°C | ASTM D150 | 4.5 – 5.0 | – |
Loss Factor | 25°C | ASTM D150 | 100 – 130 x 10⁻³ | – |
Volume Resistivity | 25°C | ASTM D257 | 3.0 x 10¹⁴ – 5.0 x 10¹⁴ | Ω·cm |
Dielectric Strength | 25°C | ASTM D149 | 21 – 24 | kV/mm |
Tensile Strength | – | ASTM D638 | 4 – 6 | MN/m² |
Elongation at Break | – | ASTM D638 | 50 – 60 | % |